WEKO3
アイテム
{"_buckets": {"deposit": "e67a718b-faff-49d8-add5-9767c8984998"}, "_deposit": {"created_by": 3, "id": "3847", "owners": [3], "pid": {"revision_id": 0, "type": "depid", "value": "3847"}, "status": "published"}, "_oai": {"id": "oai:tobunken.repo.nii.ac.jp:00003847", "sets": ["525"]}, "author_link": ["15765", "15767", "15768", "15771", "15766", "15770", "15764", "15763", "15762", "15769"], "item_10001_biblio_info_7": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "2012-03-31", "bibliographicIssueDateType": "Issued"}, "bibliographicIssueNumber": "51", "bibliographicPageEnd": "312", "bibliographicPageStart": "303", "bibliographic_titles": [{"bibliographic_title": "保存科学"}, {"bibliographic_title": "Science for conservation", "bibliographic_titleLang": "en"}]}]}, "item_10001_description_5": {"attribute_name": "抄録", "attribute_value_mlt": [{"subitem_description": " Hagia Sophia has been suffering from salt crystallization and flaking of the wall surface,especially at the northwest part of the building. Therefore,a survey was conducted with the following aims:\n 1. To identify the crystalized salts in Hagia Sophia\n 2 .To clarify the origin of salt and the movement of water which is the main cause of salt crystallization\n 3. To make a suggestion for the future conservation program,including salt and water control.\n Elements containing salt samples were detected by X-ray fluorescence spectroscopy, and crystallized molecules were identified by X-ray diffraction analysis.\n As a result,the types of crystallized salt were identified as sodium sulfate,magnesium sulfate and sodium nitrate. At the northwest part of the building (northwest exedra), the major type of salt is sodium sulfate;magnesium sulfate and sodium nitrate were found at\nthe western and northern parts of the exedra where salt crystallization is in progress. The removal of plaster from the outer wall surface and the infiltration of rainwater from the exposed wall are thought to be the causes of deterioration at the northwest part of the building.", "subitem_description_type": "Abstract"}]}, "item_10001_identifier_registration": {"attribute_name": "ID登録", "attribute_value_mlt": [{"subitem_identifier_reg_text": "10.18953/00003837", "subitem_identifier_reg_type": "JaLC"}]}, "item_creator": {"attribute_name": "著者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "佐々木, 淑美"}], "nameIdentifiers": [{"nameIdentifier": "15762", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "吉田, 直人"}], "nameIdentifiers": [{"nameIdentifier": "15763", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "小椋, 大輔"}], "nameIdentifiers": [{"nameIdentifier": "15764", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "石﨑, 武志"}, {"creatorName": "[石崎, 武志]", "creatorNameLang": "ja-Kana"}], "nameIdentifiers": [{"nameIdentifier": "15765", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "日高, 健一郎"}], "nameIdentifiers": [{"nameIdentifier": "15766", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Juni, SASAKI", "creatorNameLang": "en"}], "nameIdentifiers": [{"nameIdentifier": "15767", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Naoto, YOSHIDA", "creatorNameLang": "en"}], "nameIdentifiers": [{"nameIdentifier": "15768", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Daisuke, OGURA", "creatorNameLang": "en"}], "nameIdentifiers": [{"nameIdentifier": "15769", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Takeshi, ISHIZAKI", "creatorNameLang": "en"}], "nameIdentifiers": [{"nameIdentifier": "15770", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Kenichiro, HIDAKA", "creatorNameLang": "en"}], "nameIdentifiers": [{"nameIdentifier": "15771", "nameIdentifierScheme": "WEKO"}]}]}, "item_files": {"attribute_name": "ファイル情報", "attribute_type": "file", "attribute_value_mlt": [{"accessrole": "open_date", "date": [{"dateType": "Available", "dateValue": "2017-07-31"}], "displaytype": "detail", "download_preview_message": "", "file_order": 0, "filename": "05125.pdf", "filesize": [{"value": "2.9 MB"}], "format": "application/pdf", "future_date_message": "", "is_thumbnail": false, "licensetype": "license_11", "mimetype": "application/pdf", "size": 2900000.0, "url": {"label": "05125.pdf", "url": "https://tobunken.repo.nii.ac.jp/record/3847/files/05125.pdf"}, "version_id": "414d365a-38d9-4c35-b14f-2b3e1c007a65"}]}, "item_keyword": {"attribute_name": "キーワード", "attribute_value_mlt": [{"subitem_subject": "塩の析出", "subitem_subject_scheme": "Other"}, {"subitem_subject": "剥離", "subitem_subject_scheme": "Other"}, {"subitem_subject": "雨水の浸透", "subitem_subject_scheme": "Other"}, {"subitem_subject": "外壁面からの漆喰の除去", "subitem_subject_scheme": "Other"}, {"subitem_subject": "ハギア", "subitem_subject_scheme": "Other"}, {"subitem_subject": "ソフィア大聖堂", "subitem_subject_scheme": "Other"}, {"subitem_subject": "析出塩類", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Hagia Sophia; salt crystallization; flaking; infiltration of rainwater; removal of the plaster from outer wall", "subitem_subject_language": "en", "subitem_subject_scheme": "Other"}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "jpn"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "journal article", "resourceuri": "http://purl.org/coar/resource_type/c_6501"}]}, "item_title": "〔報告〕ハギア・ソフィア大聖堂内壁の析出塩類の調査", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "〔報告〕ハギア・ソフィア大聖堂内壁の析出塩類の調査"}, {"subitem_title": "Study of Salt Crystallization on the Inner Wall of Hagia Sophia, Istanbul, Turkey", "subitem_title_language": "en"}]}, "item_type_id": "10001", "owner": "3", "path": ["525"], "permalink_uri": "https://doi.org/10.18953/00003837", "pubdate": {"attribute_name": "公開日", "attribute_value": "2017-07-31"}, "publish_date": "2017-07-31", "publish_status": "0", "recid": "3847", "relation": {}, "relation_version_is_last": true, "title": ["〔報告〕ハギア・ソフィア大聖堂内壁の析出塩類の調査"], "weko_shared_id": 3}
〔報告〕ハギア・ソフィア大聖堂内壁の析出塩類の調査
https://doi.org/10.18953/00003837
https://doi.org/10.18953/00003837f5221044-e18a-4b64-be77-6a841561a49b
名前 / ファイル | ライセンス | アクション |
---|---|---|
05125.pdf (2.9 MB)
|
Item type | 学術雑誌論文 / Journal Article(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2017-07-31 | |||||
タイトル | ||||||
タイトル | 〔報告〕ハギア・ソフィア大聖堂内壁の析出塩類の調査 | |||||
タイトル | ||||||
言語 | en | |||||
タイトル | Study of Salt Crystallization on the Inner Wall of Hagia Sophia, Istanbul, Turkey | |||||
言語 | ||||||
言語 | jpn | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | 塩の析出 | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | 剥離 | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | 雨水の浸透 | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | 外壁面からの漆喰の除去 | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | ハギア | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | ソフィア大聖堂 | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | 析出塩類 | |||||
キーワード | ||||||
言語 | en | |||||
主題Scheme | Other | |||||
主題 | Hagia Sophia; salt crystallization; flaking; infiltration of rainwater; removal of the plaster from outer wall | |||||
資源タイプ | ||||||
資源タイプ識別子 | http://purl.org/coar/resource_type/c_6501 | |||||
資源タイプ | journal article | |||||
ID登録 | ||||||
ID登録 | 10.18953/00003837 | |||||
ID登録タイプ | JaLC | |||||
著者 |
佐々木, 淑美
× 佐々木, 淑美× 吉田, 直人× 小椋, 大輔× 石﨑, 武志× 日高, 健一郎× Juni, SASAKI× Naoto, YOSHIDA× Daisuke, OGURA× Takeshi, ISHIZAKI× Kenichiro, HIDAKA |
|||||
抄録 | ||||||
内容記述タイプ | Abstract | |||||
内容記述 | Hagia Sophia has been suffering from salt crystallization and flaking of the wall surface,especially at the northwest part of the building. Therefore,a survey was conducted with the following aims: 1. To identify the crystalized salts in Hagia Sophia 2 .To clarify the origin of salt and the movement of water which is the main cause of salt crystallization 3. To make a suggestion for the future conservation program,including salt and water control. Elements containing salt samples were detected by X-ray fluorescence spectroscopy, and crystallized molecules were identified by X-ray diffraction analysis. As a result,the types of crystallized salt were identified as sodium sulfate,magnesium sulfate and sodium nitrate. At the northwest part of the building (northwest exedra), the major type of salt is sodium sulfate;magnesium sulfate and sodium nitrate were found at the western and northern parts of the exedra where salt crystallization is in progress. The removal of plaster from the outer wall surface and the infiltration of rainwater from the exposed wall are thought to be the causes of deterioration at the northwest part of the building. |
|||||
書誌情報 |
保存科学 en : Science for conservation 号 51, p. 303-312, 発行日 2012-03-31 |